311 Excellent High-Temperature Resistance Gold and Silver Antitarnish
Product Brief
311 is a high-performance, high-temperature resistant anti-tarnish agent developed for silver plated layers in the communication electronics industry. Its protection is verified on Cu 6 μm / Ag 1 μm deposits: silver-plated workpieces show no discoloration after 30 minutes at 280°C, and remain unchanged after 1 hour at 150°C. At the same time, the silver coating resists the 5% potassium sulfide (K₂S) test for more than 5 minutes at 25°C, while gold plating passes a 72-hour neutral salt spray test without corrosion. Bath make-up is a simple three-step operation — half volume of pure water, add the agent, top up to final volume — with a wide working concentration of 50–150 ml/L. For lines that need both sulfur resistance and true high-temperature survival, 311 removes the trade-off between the two.
Core Product Advantages
1.Best-in-Class High Temperature Resistance: 280°C for 30 Minutes
The protective film is engineered for the thermal load of modern electronics assembly. Silver-plated workpieces treated with 311 show no discoloration after 30 minutes at 280°C, and remain unchanged after 1 hour at 150°C. This covers SMT reflow soldering, high-temperature baking and downstream assembly steps, so the finish comes through the whole process without yellowing, blackening or dullness — and without the scrapping that follows a failed high-temperature test.
2.Excellent Potassium Sulfide Resistance
In the 5% potassium sulfide (K₂S) test at 25°C, silver coatings treated with 311 stay discoloration-free for more than 5 minutes — the actual duration depends on the thickness of the silver layer. It blocks sulfur ion attack from air and packaging materials, eliminating the spotting and blackening that degrade both the appearance and the contact performance of silver surfaces.
3.Long-Lasting Anti-Corrosion Protection for Gold Plating
311 isolates moisture and corrosive media in the air efficiently. Gold-plated workpieces pass the 72-hour neutral salt spray test without corrosion or spots, extending service life greatly for gold-finished parts used in humid, coastal and corrosive working conditions.
4.Verified on Thin Silver over Copper (Cu 6 μm / Ag 1 μm)
311 is specified for silver plating on copper in the communication electronics industry, and its high-temperature performance is verified on Cu 6 μm / Ag 1 μm deposits — the thin silver build typical of connectors, terminals and RF parts. Where the deposit is thin there is no room for a weak protective layer, and 311 is validated at exactly that build.
Wide Application Industries & Workpieces
1.Silver-Plated Connectors & Terminals for Communication Equipment
Suitable for copper substrates with thin silver plating used in communication connectors, signal terminals and conductive components. The film holds up through reflow and high-temperature assembly while preventing silver blackening during long-term storage and outdoor service.
2.Silver-Plated Contacts for Precision Relays & Switches
Designed for thin silver-plated moving/static contacts and switch shrapnel. It enhances the anti-tarnish capacity of thin silver coatings, prevents contact resistance drift and ensures stable, sensitive electrical signal transmission.
3.Silver-Plated RF Cavities & Antenna Components
Ideal for silver-plated RF cavities, antenna assemblies and industrial parts that see high temperature in service or in downstream processing. It satisfies the dual demands of sulfur resistance and high temperature resistance in one treatment.
4.Gold & Silver Pads on PCB Circuit Boards
Specially formulated for the anti-corrosion and anti-tarnish protection of PCB gold-plated and partially silver-plated pads. It solves gold surface corrosion in humid environments while preserving an even, clean appearance.
5.Silver-Plated Parts Subject to SMT Reflow Soldering
For workpieces that must pass through reflow or high-temperature baking after plating, 311 keeps the silver surface bright and sulfur-resistant, avoiding the mass scrapping caused by high-temperature discoloration.



Solution Composition & Operating Parameters
|
Parameter |
Working Range |
Optimum |
|
311 Concentration |
50 - 150 ml/L |
100 ml/L |
|
Operating Temperature |
55 - 65 ℃ |
60 ℃ |
|
Soaking Time |
5 - 20 min |
10 min |
Note: If the anti-tarnish agent has solidified into a paste-like solid during storage, simply place the container in an 80℃ water bath until the concentrate melts completely into a uniform, semi-transparent liquid.
Bath Make-up
1.Fill the working tank with 50% of the final volume of pure water.
2.Add the 311 anti-tarnish agent.
3.Top up with pure water to the final volume.
Complete Process Flow
Process sequence: Silver Plating → Pure Water Rinse → 311 Anti-Tarnish Dip → Pure Water Rinse → Drying
1、Anti-Tarnish Dipping
Immerse the plated workpieces in the prepared 311 working solution. Immersion time is 5–20 minutes, with 10 minutes as the optimum.
2、Pure Water Rinsing
Take out the dipped workpieces and rinse them in pure water.
3、Drying
Dry the rinsed workpieces.
Equipment
Tank: PP / PE
Heater: quartz heater
Agitation: mechanical agitation
Solution Analysis
Reagents: phenolphthalein indicator; 1N NaOH solution.
Procedure:
1.Pipette 100 ml of the 311 working solution into a 200 ml conical flask.
2.Add 3–6 drops of phenolphthalein indicator.
3.Titrate with 1N NaOH solution until the colour changes from colourless to light pink, then stop.
Calculation: 311 (%) = 1N NaOH consumed (ml) × 3.84 − 0.36
Precautions
The working solution must be circulated and heated on site; never allow local overheating. The working temperature must be based on actual measurement — do not rely on the temperature shown on the heating tube.
Product Performance Test Data
- Silver Plating K₂S Resistance Test: No discoloration for over 5 minutes in 5% potassium sulfide solution at 25°C (duration related to silver coating thickness)
- High Temperature Resistance Test: No discoloration after 1 hour at 150°C
- High Temperature Resistance Test: No discoloration after 30 minutes at 280°C (Cu 6 μm / Ag 1 μm deposits)
- Gold Plating Salt Spray Test: No corrosion after a 72-hour neutral salt spray test
Storage Instructions
Store the product under dry and cool conditions with the temperature maintained between 5℃ and 35℃. Do not place it where it is exposed to direct sunlight. Use the product within its valid shelf life for optimal performance.