343 Excellent Potassium Sulfide Resistance Gold and Silver Antitarnish
Product Brief
Core Product Advantages
1.Industry-Leading Potassium Sulfide Resistance
Conventional silver anti-tarnish agents turn black within 30 seconds to 3 minutes in 5% K2S solution, while 343 delivers superior anti-sulfur performance. At 25°C room temperature, silver coatings stay discoloration-free for 3–15 minutes, and longer protection is achieved with thicker silver plating. It effectively blocks sulfur ion erosion from air and packaging materials to eliminate spotting and blackening of gold and silver surfaces.
2.High Temperature Anti-Tarnish Property Compatible with SMT Reflow Soldering
The protective film features stable high-temperature resistance. Silver-plated workpieces treated with 343 stay clean and bright after 10 minutes baking at 260°C, without yellowing, blackening or dullness. It fully adapts to post-processes such as SMT reflow soldering and high-temperature assembly, avoiding mass product scrapping caused by high-temperature discoloration.
3.Long-Lasting Anti-Corrosion Protection for Gold Plating
343 isolates moisture and corrosive media in the air efficiently. Gold-plated workpieces treated with 343 pass the 72-hour neutral salt spray test without corrosion or spots, extending service life greatly for gold products used in humid, coastal and corrosive working conditions.
4. Optional Electrolytic Treatment for Higher Performance Requirements
Beyond simple immersion, 343 can also be used with electrolysis when higher performance is required. Stainless steel or titanium mesh can be used as the anode, with the voltage set at 2–3V — a flexible option that lets customers add an extra margin of protection without changing the basic process.
Wide Application Industries & Workpieces
1.Silver-Plated Connectors for New Energy & Communication
Suitable for copper substrates pre-nickel plated and bright silver-plated automotive connectors, signal terminals and communication conductive components. It prevents silver layer blackening during long-term storage and outdoor service to guarantee stable conductive performance.
2.Silver Contacts for Precision Relays & Switches
Designed for thin silver-plated moving/static contacts and switch shrapnel. It enhances the anti-tarnish capacity of thin silver coatings, prevents contact resistance drift and ensures stable, sensitive electrical signal transmission.
3.High-End Silver Jewelry & Decorative Crafts
Compatible with 925 silver ornaments, electroplated silver artworks and metal decorative parts. It blocks sulfide from rubber packaging and ambient air to avoid spotted blackening, maintains long-term mirror brightness and reduces after-sales return rates.
4.Gold & Silver Pads on PCB Circuit Boards
Specially formulated for the anti-corrosion and anti-tarnish protection of PCB gold-plated and partially silver-plated pads. It solves gold surface corrosion in humid environments while preserving an even, clean appearance.
5.High-Temperature Resistant Silver-Plated RF Components
Ideal for thick silver-plated RF cavities, antenna assemblies and industrial parts operating under high-temperature conditions. It satisfies the dual protection demands of sulfur resistance and high temperature resistance for complex harsh industrial environments.



Solution Composition & Operating Parameters
|
Parameter |
Working Range |
Optimum |
|
343 Concentration |
80 - 150 ml/L |
100 ml/L |
|
Operating Temperature |
55 - 65 ℃ |
60 ℃ |
|
pH Value |
-- |
2.0 |
|
Soaking Time |
Over 5 minutes |
Per actual requirements |
Note: In winter, white lumpy precipitate may appear at low temperature. This is a normal physical change — warm the container in a 40–60℃ water bath, shake well, and use as normal.
Solution Preparation
1.Shake the anti-tarnish agent well before use. Fill a clean working tank with 2/3 of the calculated volume of pure water and heat it to 40℃.
2.Add the anti-tarnish agent slowly under gentle stirring and mix it evenly.
3.Top up to the normal working level, adjust to the operating temperature, and the solution is ready for use.
Note: Avoid heating too fast or overheating. A temperature above 80℃ may deactivate the anti-tarnish agent.
Complete Process Flow
1、Anti-Tarnish Dipping
Immerse fully cleaned workpieces in the prepared 343 working solution for about 5 minutes. Workpieces can be wet or dried before dipping, but thorough cleaning is mandatory.
2、Rinsing
Take out dipped workpieces and rinse them in room-temperature clean water; the rinsing time should not be too long — 0.5–1 minute is recommended. If low water temperature causes poor surface appearance, slightly heating the rinse water will improve the finish.
3、Draining & Drying
Drain or spin dry the rinsed workpieces, spread them out in a clean place, then blow-dry or oven-dry below 65℃.
4、Electrolytic Treatment (For Enhanced Performance)
To meet higher performance requirements, 343 can also be used with electrolysis. Stainless steel or titanium mesh can be used as the anode, with the voltage set at 2–3V.
Equipment
Tank: PP / PE
Heater: quartz heater
Agitation: mechanical agitation
Solution Maintenance
1.The working solution must be circulated and heated on site; never allow local overheating. The working temperature must be based on actual measurement — do not rely on the temperature shown on the heating tube.
2.After the solution cools down, a small amount of white precipitate may appear on the surface or on the tank wall. It disappears after slight heating and does not affect performance.
3.When not in use, both the prepared working solution and the concentrated agent must be kept covered, sealed and away from light, so that dust or foreign matter cannot affect the solution quality and protection effect.
4.If the working solution has been left unused for a long time, add an appropriate amount of pure water to compensate for evaporation and restore the original volume before reusing it.
5.Bath life varies with workpiece throughput and frequency of use, which carry in water and consume the active ingredients at different rates. The active content of the agent is always changing dynamically, so the bath must be monitored and maintained accordingly.
6.To extend the service life of the working solution, installing a circulating filtration unit is recommended. Installing an aeration (air bubbling) device is not recommended.
7.If the potassium sulfide resistance of a silver coating declines, consider neutralizing the silver coating with a weak acid, then dipping it in the silver anti-tarnish agent again.
Product Performance Test Data
● Silver Plating K2S Resistance Test: No discoloration for 3–15 minutes in 5% potassium sulfide solution at 25°C (duration related to silver coating thickness)
● High Temperature Resistance Test: No discoloration after 10 minutes baking at 260°C
● Gold Plating Salt Spray Test: No corrosion after a 72-hour neutral salt spray test
● K2S Grade Selection: Potassium sulfide is available on the market at 45%, 50% and 98% content, as well as blackening grades of unknown content. To ensure the accuracy of K2S test results, 98% content is recommended.
Storage Instructions
Store the product in a clean, dry place with the temperature maintained between 5℃ and 35℃. Do not place it where it is exposed to direct sunlight. Use the product within its valid shelf life for optimal performance.
Note: For the relationship between temperature and the potassium sulfide test result, please refer to the temperature–K2S test correlation chart.