Leave Your Message

Low‑dosage easy‑to‑operate protection WST Gold and Silver Antitarnish

WST Excellent Potassium Sulfide Resistance Gold and Silver Antitarnish is a water-based anti-tarnish agent for gold & silver plating. Silver coating withstands 5% K2S test for 3–20 mins at 25°C and 260°C high temp for 10 mins without discoloration; gold plating passes 72hrs neutral salt spray test. Near-neutral pH 7.0 working bath, simple immersion process. Factory direct export for connectors, PCB, silver jewelry, precision electronic components.

    Product Brief

    ▪ WST is a high-performance anti-tarnish agent developed exclusively for electroplated gold and silver layers. For silver coatings: it keeps the surface discoloration-free for 3–20 minutes under the 5% potassium sulfide (K2S) test at 25°C (the anti-tarnish duration positively correlates with silver coating thickness), and shows no discoloration after 10 minutes baking at 260°C. For gold plating: it delivers full protection against corrosion during a 72-hour neutral salt spray test. The working solution runs at a near-neutral pH of 7.0 with a wide working concentration of 30–80 ml/L. Applied by simple immersion, WST fits easily into existing plating lines — a PP/PE tank, a quartz heater and mechanical agitation are all that is needed. It is a reliable choice for gold and silver plated workpieces that must retain their appearance and performance through long-term storage and service.

    Core Product Advantages

    1.Industry-Leading Potassium Sulfide Resistance

    Conventional silver anti-tarnish agents turn black within 30 seconds to 3 minutes in 5% K2S solution, while WST delivers superior anti-sulfur performance. At 25°C room temperature, silver coatings stay discoloration-free for 3–20 minutes, and longer protection is achieved with thicker silver plating. It effectively blocks sulfur ion erosion from air and packaging materials to eliminate spotting and blackening of gold and silver surfaces.

    2.High Temperature Anti-Tarnish Property Compatible with SMT Reflow Soldering

    The protective film features stable high-temperature resistance. Silver-plated workpieces treated with WST stay clean and bright after 10 minutes baking at 260°C, without yellowing, blackening or dullness. It fully adapts to post-processes such as SMT reflow soldering and high-temperature assembly, avoiding mass product scrapping caused by high-temperature discoloration.

    3.Long-Lasting Anti-Corrosion Protection for Gold Plating

    WST isolates moisture and corrosive media in the air efficiently. Gold-plated workpieces treated with WST pass the 72-hour neutral salt spray test without corrosion or spots, extending service life greatly for gold products used in humid, coastal and corrosive working conditions.

    4.Near-Neutral pH 7.0 Working Bath with a Wide Operating Window

    The WST working solution runs at pH 7.0 — a near-neutral condition rather than a strongly acidic one. Combined with a wide working concentration of 30–80 ml/L (optimum 50 ml/L) and an operating temperature window of 55–65℃, it gives the production line a comfortable margin for stable, repeatable anti-tarnish results.

    Wide Application Industries & Workpieces

    1.Silver-Plated Connectors for New Energy & Communication

    Suitable for copper substrates pre-nickel plated and bright silver-plated automotive connectors, signal terminals and communication conductive components. It prevents silver layer blackening during long-term storage and outdoor service to guarantee stable conductive performance.

    2.Silver Contacts for Precision Relays & Switches

    Designed for thin silver-plated moving/static contacts and switch shrapnel. It enhances the anti-tarnish capacity of thin silver coatings, prevents contact resistance drift and ensures stable, sensitive electrical signal transmission.

    3.High-End Silver Jewelry & Decorative Crafts

    Compatible with 925 silver ornaments, electroplated silver artworks and metal decorative parts. It blocks sulfide from rubber packaging and ambient air to avoid spotted blackening, maintains long-term mirror brightness and reduces after-sales return rates.

    4. Gold & Silver Pads on PCB Circuit Boards

    Specially formulated for the anti-corrosion and anti-tarnish protection of PCB gold-plated and partially silver-plated pads. It solves gold surface corrosion in humid environments while preserving an even, clean appearance.

    5.High-Temperature Resistant Silver-Plated RF Components

    Ideal for thick silver-plated RF cavities, antenna assemblies and industrial parts operating under high-temperature conditions. It satisfies the dual protection demands of sulfur resistance and high temperature resistance for complex harsh industrial environments.

    Low‑dosage easy‑to‑operate protection WST Gold and Silver Antitarnish-1(1)
    Low‑dosage easy‑to‑operate protection WST Gold and Silver Antitarnish-2(1)
    Low‑dosage easy‑to‑operate protection WST Gold and Silver Antitarnish-3(1)

    Solution Composition & Operating Parameters

    Parameter

    Working Range

    Optimum

    WST Concentration

    30 - 80 ml/L

    50 ml/L

    Operating Temperature

    55 - 65 ℃

    60 ℃

    pH Value

    ---

    7.0

    Soaking Time

    Over 5 minutes

    ---

    Note: If the storage temperature is below 30℃, the concentrated agent solidifies into a paste-like solid. This is reversible — warm the container in an 80℃ water bath until it melts completely into a uniform, semi-transparent liquid before use.

    Solution Preparation

    1.Shake the anti-tarnish agent well before use. If the storage temperature is below 30℃, the agent solidifies into a paste-like solid; simply place the container in an 80℃ water bath until the concentrate melts completely into a uniform, semi-transparent liquid.

    2.Fill a clean working tank with the calculated volume of pure water and heat it to 40℃.

    3.Add the uniform, semi-transparent anti-tarnish agent slowly under gentle stirring and mix it evenly.

    4.Adjust to the operating temperature, and the solution is ready for use.

    Note: Avoid heating too fast or overheating. A temperature above 80℃ may deactivate the anti-tarnish agent.

    Complete Process Flow

    1、Anti-Tarnish Dipping

    Immerse fully cleaned workpieces in the prepared WST working solution for about 5 minutes. Workpieces can be wet or dried before dipping, but thorough cleaning is mandatory.

    2、Rinsing

    Take out dipped workpieces and rinse them in room-temperature clean water; the rinsing time should not be too long — 0.5–1 minute is recommended. If low water temperature causes poor surface appearance, slightly heating the rinse water will improve the finish.

    3、Draining & Drying

    Drain or spin dry the rinsed workpieces, spread them out in a clean place, then blow-dry or oven-dry below 65℃.

    Equipment

    Tank: PP / PE

    Heater: quartz heater

    Agitation: mechanical agitation

    Solution Maintenance

    1.The anti-tarnish agent must be heated in a water bath until it turns transparent before use. On site the working solution must be circulated and heated; never allow local overheating. The working temperature must be based on actual measurement — do not rely on the temperature shown on the heating tube.

    2.After the solution cools down, a small amount of white precipitate may appear on the surface or on the tank wall. It disappears after slight heating and does not affect performance.

    3.When not in use, both the prepared working solution and the concentrated agent must be kept covered, sealed and away from light, so that dust or foreign matter cannot affect the solution quality and protection effect.

    4.If the working solution has been left unused for a long time, add an appropriate amount of pure water to compensate for evaporation and restore the original volume before reusing it.

    5.Bath life varies with workpiece throughput and frequency of use, which carry in water and consume the active ingredients at different rates. The active content of the agent is always changing dynamically, so after the bath has been in service for some time, top it up with concentrated agent or replace the bath according to the sulfide resistance required by the parts.

    6.To extend the service life of the working solution, installing a circulating filtration unit is recommended.

    7.If the potassium sulfide resistance of a silver coating declines, consider neutralizing the silver coating with a weak acid, then dipping it in the silver anti-tarnish agent again.

    Product Performance Test Data

    ● Silver Plating K2S Resistance Test: No discoloration for 3–20 minutes in 5% potassium sulfide solution at 25°C (duration related to silver coating thickness)

    ● High Temperature Resistance Test: No discoloration after 10 minutes baking at 260°C

    ● Gold Plating Salt Spray Test: No corrosion after a 72-hour neutral salt spray test

    ● K2S Grade Selection: Potassium sulfide is available on the market at 45%, 50% and 98% content, as well as blackening grades of unknown content. To ensure the accuracy of K2S test results, 98% content is recommended.

    Storage Instructions

    Store the product in a clean, dry place with the temperature maintained between 5℃ and 35℃. Do not place it where it is exposed to direct sunlight. Use the product within its valid shelf life for optimal performance.

    Leave Your Message